PHYSICAL PROPERTIES OF MORTARS & BRICKS AS PER IS SPECIFICATIONS

Furan Resin Mortar Bitumen Primer Bitumor Mastic Silimor Silicate K. Mortar Silimor Silicate Mortar Sulphur Mortar Phenolic Resin Mortar Epoxy Mortar Polyester Mortar A.R, Bricks Class - 1
1 Working time [ Minutes] 20 Minutes     20 minutes 15 minutes - 20 Minutes 20 Minutes (Min) 20 Minutes (Min)  
2. Flexural strength 75 Kg/cm2     40 Kg/cm2 35 Kg/cm2 70 Kg/cm2 75 Kg/cm2 150 Kg/cm2 150 Kg/cm2 100 Kg/cm2
3. Compressive Strength 350 Kg/cm2     150 Kg/cm2 100 Kg/cm2 280 Kg/cm2 350 Kg/cm2
500 Kg/cm 500 Kg/cm2 700 Kg/cm2
4. Bond Strength 10 kg/cm2     5 Kg/cm2 5 Kg/cm2 10 Kg/cm2 10 Kg/cm2 10 Kg/cm2 12 Kg/cm2  
5. Absorption bye weight 1% Max     Tolune absorption max 18% Tolune absorption max 18% Max. 1% Max. 1% Max. 1% Max 1% Max 2%
6. Drying time   Not More than 8 hrs Density of Primer 0.86 grm/cc                
7. Hardnest number     4 to 12 at 35°C              
8. Bitumen contents in Mastic     13% to 18%              
9. % of Aggregate in mastic     82% to 87%